产品介绍
At temperatures above 2012° F (1100° C), graphite dust from graphite liners\/shields or heating elements can attack and carburize molybdenum sheaths. This causes the sheath to crystallize and become porous, losing its protective properties. The thermal elements in turn crystallize and open. Coating the heat-affected length of the molybdenum sheath with a thick layer of tungsten reduces this carburization action and extends probe life. The tungsten coating also provides increased abrasion resistance.
Tungsten-Coated Molybdenum for Graphite-Lined Furnaces 热电偶温度探头技术参数
点击查看 0 个替代产品
规格项 | 参数值 | 勾选搜索替代 |
特 性 | ||
结构类型 | Ungrounded Thermocouple | |
特征 | Available as an Assembly | |
连 接 & 显 示 | ||
连接方式 | Threaded Fitting | |
物 理 | ||
探头配置 | Straight Probe | |
直径或宽度 | 0.1250 to 0.3750 inch (3.17 to 9.52 mm) | |
更多规格 | ||
金属、贵金属和难熔金属类型 | S (optional feature) | |
产品类别 | Thermocouple Temperature Probes | |
护套材料 | Tungsten-Coated Molybdenum |